Casting Study: Metal Saw Handle Frame
This product has been created for a top quality, guaranteed-for-life hacksaw. Zinc alloys satisfy the surface coating and the mechanical resistance required for the handle and saw blade guide, with the process economy for a high-quality product on a competitive market. This can be contributed to the long life of the dies and tooling for very high-volume production. The rigidity of the assembly ensured by the zinc alloy allows the blade to be stressed safely up to 140 kg traction force.