antenna LNB die casting

Antenna LNB/Feedhorn Assembly

View

Feedhorn incorporates six graphite permanent mold castings, including the end cap, housing (which holds the circuit boards), feedhorn, cover (used for shielding), and two mounting probes. ZA-12 alloy provides the components with the necessary strength to withstand the...

Control Handles and Mounting Box

View

ZA-12 graphite permanent mold castings are used for the gunner’s control handles and mounting box because the process is an economical low-volume casting method. ZA-12 also provides the handles with the density to simulate steel. Graphite permanent mold casting is...
4a2_photo2_caseID135

Foot Switch – Control International

View

Over time, the costs associated with machining the cast-iron switch cover eroded manufacturing margins. The decision was then made to zinc die cast the cover. Zinc had the density and weight Control International specified, and it provided better fit, quality, and...
gearho2_photo2_caseID138

Gear Housing

View

Engineers decreased time-to-market by utilizing existing gear housing tooling to develop a higher load winch. Superwinch’s 1,500-lb. unit incorporated two 380 Aluminium die cast housings which functioned as rotating and stationary ring gears. By substituting ZA-27...
hammerc2_photo2_caseID81

Hammer Cap

View

Operating at pressures ranging from 50 to 125 psi, the Danair Aerosmith hammer delivers up to 1,000 hammer blows per minute. During the early production phase finish machining exposed casting porosity and the cast iron air grille vents frequently broke during service....
handlef2_photo2_caseID85

Handle for Electrical Cabinet

View

This zinc alloy part is designed to raise the global quality perception of the final product. The dimensional precision of the process for the fine fitting of different sub assemblies and the long life of the mold and tooling for large production series led the choice...
housinf2_photo2_caseID89

Housing & Frame

View

The elements of this equipment (TYCAS) were created to detect the positions of approaching aircraft according to new security norms of the IATA. The process proved to be more economical compared to traditional machining despite limited series and to pressure die cast...
housinb2_photo2_caseID90

Housing and Base Plate

View

Originally, the housing and base plate frame were sand cast aluminium and finish machined. Machining and assembly time took 3.5 hours per unit. During a redesign, the company set about to reduce costs without sacrificing quality or performance. This led to graphite...
metalsa2_photo2_caseID105

Metal Saw Handle Frame

View

This product has been created for a top quality, guaranteed-for-life hacksaw. Zinc alloys satisfy the surface coating and the mechanical resistance required for the handle and saw blade guide, with the process economy for a high-quality product on a competitive...

PC-Gehäuse zur Montage auf der Hutschiene

View

Die PC-Gehäuse Bauteile mussten vielfältige Anforderungen erfüllen: Neben Robustheit beim Handling in industrieller Umgebung und einer hochwertigen Optik zählten eine optimale Wärmeabfuhr und abschirmende Eigenschaften zu den Kriterien, die letztlich für Zink als...

Planter Handler

View

The planter handle is used to adjust spring force to a pair of closing wheels. It is important for the handle to be durable, easily accessible, and very comfortable to grip. To accent product appearance, designers chose a die cast over a welded fabrication. Die cast...
ratchet2_photo2_caseID144

Ratchet Housing

View

The goal of product designers for the 1/4 in. air ratchet was to lower product manufacturing costs while improving performance and appearance. The original product design specified an axial assembly–a machined steel head attached by a lock nut to a housing handle....
trimfra2_photo2_caseID156

Trim Frame

View

The instrument incorporates two frames, one for the front panel and another in the rear. Originally the frames were designed as welded aluminium extrusions. In search of alternative methods, the manufacturer looked to zinc graphite permanent mould casting with its low...

Two-Piece Housing

View

When Black & Decker decided to introduce a new manual staple gun, designers and engineers started with a clean slate. Their goal was to integrate efficiency, simplicity, and ergonomics into the new tool. The result is a radical design that moves the handle pivot...
visecom2_photo2_caseID160

Vise Components

View

Eight separate ZA-12 alloy castings are utilized in the TUCKER woodworking vise. Castings form the pivot block, front jaw, rear jaw, quick-release nut, yoke, stanchion, mounting plate, and keeper plate. Based on the shapes needed to form the vise, casting easily...