Bolt Guide – Remington Powerhammer

View

A value analysis on the Remington Powerhammer targeted the bolt guide for cost reduction. The bolt guide was originally designed as a screw machined steel component. After prototyping and testing, engineers decided that die casting and ZA-8 provide the design...
checkva2_photo2_caseID73

Check Valve

View

Previously, the check valve was assembled from machined aluminium bar stock and brass pipe fittings. A net shape die casting was designed by consolidating the six-piece assembly into a single, net shape component. All holes and seven thread sets, including a male...
gearcac2_photo2_caseID176

Gear Case (III)

View

Wen Products designed a new line of jig and pruning saws which required a rugged gear drive. This drive utilizes a complex case design which mounts to the motor, houses the drive gears, and guides the reciprocating blade. The case also provides the required spacing...

Getriebegehäuse

View

Für das Getriebegehäuse eines Hochdruckreinigers wurde bei einem Zinkdruckgussteil aus der laufenden Produktion durch eine konstruktive Überarbeitung bei gleicher Funktion eine Gewichtsreduzierung um 22 Prozent erzielt. Neben der Material- und Energieersparnis wurde...
hammerc2_photo2_caseID81

Hammer Cap

View

Operating at pressures ranging from 50 to 125 psi, the Danair Aerosmith hammer delivers up to 1,000 hammer blows per minute. During the early production phase finish machining exposed casting porosity and the cast iron air grille vents frequently broke during service....
ima09

Housing for electro-tool

View

The drive head of this tool, made out of 2 parts, is cast in ZP5.  This casing contains the gear that translates rotating and oscillating movements at very high rpm and frequencies. The part needed to comply with low tolerances for shape and position in both...
lawnedg2_photo2_caseID96

Lawn Edge Trimmer

View

The innovative Qualcast Lawn Edge Trimmer, the design of which is patented, is entirely based on zinc castings, which are used for both drive train and housings. The trimmer is attached to the standard Concorde mower by replacing the existing belt drive cover with a...
6b2_photo2_caseID104

Lubrication Metering Assembly – Graco, Inc.

View

The design requirements for the assembly’s 10-in.-long housing called for non-tapered walls in the meter chamber, allowing free rotation of the metering gears and zero draft in the valve area. Previous designs utilized two aluminum castings requiring secondary...
metalsa2_photo2_caseID105

Metal Saw Handle Frame

View

This product has been created for a top quality, guaranteed-for-life hacksaw. Zinc alloys satisfy the surface coating and the mechanical resistance required for the handle and saw blade guide, with the process economy for a high-quality product on a competitive...
lasermt2_photo2_caseID107

Microscan Systems – VS 310 Scanner

View

Designers of an ultra-compact scanner needed to reduce the internal envelope. The optics bracket was one component that was reduced in size but increased in functionality. The goal was to design a single mounting bracket that would accommodate a laser module, a...
ratchet2_photo2_caseID144

Ratchet Housing

View

The goal of product designers for the 1/4 in. air ratchet was to lower product manufacturing costs while improving performance and appearance. The original product design specified an axial assembly–a machined steel head attached by a lock nut to a housing handle....
regula2_photo2_caseID184

Regulator

View

The regulator for Turner’s self-igniting torch has a design criteria specifying pressure tightness, strength, cleanliness and metal-chip free, net shape, and cost-effective manufacturing. A screw-machined aluminium or brass regulator was first considered, but both...

Two-Piece Housing

View

When Black & Decker decided to introduce a new manual staple gun, designers and engineers started with a clean slate. Their goal was to integrate efficiency, simplicity, and ergonomics into the new tool. The result is a radical design that moves the handle pivot...

Two-Piece Punch Body

View

For three generations, B-V has been producing heavy-duty, specialty hand punches from two sand-cast malleable iron halves. Sand casting inaccuracies required sorting and extensive fitting to locate matching halves. Thickness variations up to 0.025 in. were...
visecom2_photo2_caseID160

Vise Components

View

Eight separate ZA-12 alloy castings are utilized in the TUCKER woodworking vise. Castings form the pivot block, front jaw, rear jaw, quick-release nut, yoke, stanchion, mounting plate, and keeper plate. Based on the shapes needed to form the vise, casting easily...
xraytan2_photo2_caseID161 (1)

X-ray tank+lock+guide Tube Assembly

View

The X-ray tank + lock + guide assembly consists of a very high frequency generator for dental radiology. The parts in this assembly are made of pressure die cast Zamak 5 (ZA4IUG), an alloy which offers the following functions for this application: mechanical strength,...