Casting Study: Precision Plate ensuring smooth movements of the robot on X and Y axes
This part, which replaced a machined steel part, required precision tolerances for the diameter of the bores and the spacing between them. Zinc casting also provided the required dimensional stability over time and permitted this complex shape to be cast in one piece that also contributed to the rigidity of the assembly.