Search Casting Studies



There are 9 studies matching your search criteria.

ima08

Central Support Unit

View

This part is a central support unit for mounting all optical, electrical, and mechanical components for the imaging plate technology in use in dentistry. In medical technology, die cast zinc has been used for many years; however, overall, this area of ​​application is...
4a2_photo2_caseID135

Foot Switch – Control International

View

Over time, the costs associated with machining the cast-iron switch cover eroded manufacturing margins. The decision was then made to zinc die cast the cover. Zinc had the density and weight Control International specified, and it provided better fit, quality, and...
ima07

High Tension Cage

View

This part is a device component warranting the operators security during intervention on high-tension lines. The reasons behind choosing zinc alloy include the product’s complex tool design, the combination of thin wall casting and rigidity, and the dimensional...
lowspee2_photo2_caseID103

Low-Speed, High-Load Bearings

View

The Champion Series IV grader incorporates ZA-12 alloy low-speed, high load bearing to improve operation performance. This Front Axle Bearing application acts as a replacement for the grader’s front axle needle bearings. The original needle bearings performed well...
plate2_photo2_caseID140

Plate

View

The part is machined on guiding bores and reference faces. It substitutes for the pressed steel plate for several reasons: its high precision realized on machined diameters Ø < 0.02 mm and for the cost efficiency.  
ima06

Subframe and Carriage

View

The three parts of this design form a subassembly that measures the thickness of ophthalmic lenses before edging. The frame ensures the palpate lever guidance in the ophthalmic glass machine tool. Then, the glass is machined with the contour note during the palpate...
ima09

Support Unit for Drive

View

This product is a segment drive for imaging plate technology used in dentistry. A complex, modern, and advanced die casting enables precise and optimum shape design that is consistent with the mechanical properties of the die cast zinc alloy. In medical technology,...
ima11

Traffic Light Housing

View

Together, these two parts form a protective casing for the internal components of traffic lights. The material properties provide protection against vandalism and have much longer lifetimes than polymer materials. Due to thinner sections, they are also lighter than...