Casting Study: Dental – Occlusal Bite Holder Block

Major Selection Criteria: Complex Shape, Dimensional Precision, Good Finish, Mechanical Properties, Net Shape
Alloy: Zamak 5 (ZL5, ZL0410, ZnAI4Cu1, alloy 5)
Application Field: Scientific/Medical Instruments
Application Size: 25 -100 g
Surface Finish: E-Coat/Powder Coat
Casting Technique: Pressure Die Casting
Source: Dipl. Ing. Siegfried Müller Druckgießerei (Germany)

ima13

The medical sector is a highly demanding, niche market. The main benefit of using zinc die casting for this product is the outstanding surface quality achieved.