Base Plate and Shaft Support

View

While competitive versions rely on plastic, the Morse Controls high-end pleasure boat mechanical steering control utilises ZA-8 alloy die casting for the Command 290 base plate and shaft support. ZA-8 alloy was chosen for two reasons: superior mechanical properties...

Baugruppe Fußtüröffner

View

das Gussteil ist Teil einer Baugruppe für einen mechanischen Türöffner, der mit dem Fuß bedient wird. Berührungslose Türöffnung ist beispielsweise in Krankenhäusern oder öffentlichen Sanitäranlagen unter hygienischen Aspekten ein Gewinn. Der Einbau erfolgt in...
control2_photo2_caseID80

Control Boxes

View

The control boxes for Minn Kota electric motors went through several design phases before settling on zinc die casting as the material/process of choice. The boxes were originally sand cast aluminium and later die cast aluminium. Short tool life prompted engineers to...
ima13

Dental – Occlusal Bite Holder Block

View

The medical sector is a highly demanding, niche market. The main benefit of using zinc die casting for this product is the outstanding surface quality achieved.
doorcl2_photo2_caseID172

End Cap for a Pneumatic Door Closer

View

Alloy 3 was chosen as the end cap material because of the ease with which it is processed. Both material and tooling cost are minimized, and the product can be made with existing expertise and plant equipment. Alloy 3 castings can be produced with high dimensional...
ima03

Housing for KitchenAid Coffee Machine

View

The 9,5 kg zamak housing of this designer coffee machine is made from 8 zinc pressure die cast parts with weights between 2.2 kg and 75 g. The parts are powder coated. To avoid any bubbles during thermal curing of the paint, the parts are vacuum cast to avoid gas...
hub2_photo2_caseID110 (1)

Peerless Pull-Out Faucet – Delta

View

Initially, the hub–two intersecting cylinders–was a brazed assembly. Cylinders were screw machined from solid brass. Operations included turning, drilling, internal milling, cut-off, and rolling of one cylinder end to accept a plastic transition piece. The redesigned...
quickclamp2_photo2_caseID182

Quickclamp Air Prep System – IMI Norgren

View

A newly designed air preparation system utilizes zinc die casting for the major components of the Quickclamp(TM) assembly (as well as the bodies, bowls, and accessory parts of the filters, regulators and lubricators). Die cast zinc provides greater strength than...
slavelo2_photo2_caseID185

Slave Lock Mechanism

View

The initial design brief for the slave lock was that it had to have suitable mechanical properties to meet security door standards, have minimum design complexity, and use the most logical material for its purpose. Initially a hybrid construction was considered, using...
structu2_photo2_caseID152

Structural Components

View

The KitchenAid mixer utilizes zinc die castings for all of its structural components–the 4-1/2-quart pedestal model incorporates seven zinc castings, and the 5-quart bowl support model incorporates eight zinc castings. Zinc castings provide a number of design...
topandb2_photo2_caseID155

Top and bottom sensor plate – dollar bill changer

View

A dollar bill changer incorporated top and bottom sensor plates fabricated from welded stamped components. The weldments could not hold tolerances greater than +/- 0.020 in. In an effort to resolve dimensional instability and fit problems, the manufacturer, working...
ima11

Traffic Light Housing

View

Together, these two parts form a protective casing for the internal components of traffic lights. The material properties provide protection against vandalism and have much longer lifetimes than polymer materials. Due to thinner sections, they are also lighter than...