This two-piece holder was developed for a precision scientific instrument. Both castings have detailed features requiring tolerances of +/-0.00025 in. Extrusion could not be used because it could not hold the tolerances, while CNC and wire EDM were not cost effective. By utilising miniature zinc die castings, the instrument manufacturer procured an annual cost savings of $590,000.