This shift lever connects the shifter and the gear in ZF automotive gearboxes. This part was originally cast in aluminum but required tapping and other secondary operations in order to meet the close tolerances. Thanks to close collaboration with the customer, the...
This part was cast with Zincopor(R) technology, which resulted in a weight reduction of 25%. With an annual production rate of 235,000 part/year, this represents a 10-ton reduction of zinc alloy.
Utilizing zinc alloys to create this part allowed for outstanding control of each step and parameter involved in the full process, from design to final part to achieve, to achieve the perfect design. With die casting, the same surface quality and appearance could be...
The key benefits to this product’s design was a close cooperation between die caster and customer through a clipping system. It utilizes modern assembling technology, and because it does not involve a screw, creep is not a risk.
This casting part was originally produced in die cast aluminum. It could be produced only with disproportionate effort and high scrap rates. The parting plane in the casting could never reach the surface quality standards because at that position was a vacuum...
This part is a device component warranting the operators security during intervention on high-tension lines. The reasons behind choosing zinc alloy include the product’s complex tool design, the combination of thin wall casting and rigidity, and the dimensional...
The famous Parisian jeweler Boucheron has created a perfume with a particularly outstanding design of bottle – an enlargement of a ring. The blue cap symbolizes a cut stone, while the bottle itself is supported in a fine gold-plated ring. This part – die cast in zinc...
This chassis for a motor drive unit for an automatic opening roller door was made from several pressed metal parts prior to being designed as a zinc die casting. Die casting in zinc alloy 3 provided numerous benefits: 1.) Additional features such as pockets, the...
This set of six parts, four of which are made of Zamak, makes up a rechargeable perfume vaporizer. There are several notable characteristics of the final product that illustrate the versatility of the zinc alloy pressure die casting process: complexity of the assembly...
The three parts of this design form a subassembly that measures the thickness of ophthalmic lenses before edging. The frame ensures the palpate lever guidance in the ophthalmic glass machine tool. Then, the glass is machined with the contour note during the palpate...
This toothed wheel consists of two parts which are assembled with cast-in spigots and bolts in special steel. The parts are made in zinc alloy ZA-27, and apart from trimming, receive no machining or other finishing operations. The part is produced in two sizes, the...
Together, these two parts form a protective casing for the internal components of traffic lights. The material properties provide protection against vandalism and have much longer lifetimes than polymer materials. Due to thinner sections, they are also lighter than...