Search Casting Studies



There are 6 studies matching your search criteria.

Control Handles and Mounting Box

View

ZA-12 graphite permanent mold castings are used for the gunner’s control handles and mounting box because the process is an economical low-volume casting method. ZA-12 also provides the handles with the density to simulate steel. Graphite permanent mold casting is...
housing2_photo2_caseID91

Housing Cover and Thumbturn – Medeco STEELGUARD(tm) Lock

View

To meet market requirements, Medeco wanted to develop a new high security lock priced just below its top-of-the-line dropbolt lock. The high-end lock model is all brass. The housing cover is investment cast, and the thumbturn is a machined extrusion. As other...
ima03

Housing for KitchenAid Coffee Machine

View

The 9,5 kg zamak housing of this designer coffee machine is made from 8 zinc pressure die cast parts with weights between 2.2 kg and 75 g. The parts are powder coated. To avoid any bubbles during thermal curing of the paint, the parts are vacuum cast to avoid gas...
ima08

LEO Easy Opener

View

This design opener can open all kind of bottles without any damage and with very little effort. With its innovative patented mechanism, this tool won the Bundespreis 2016 award in Germany. ZP5 was chosen over other materials for its excellent surface finish, strength,...
wheelhse2_photo2_caseID149

Seat Belt and Wheelchair Restraint Housing

View

Originally, safety belt retractor housings were plastic injection molded. The plastic housings were easily damaged and caused retraction to malfunction. To meet performance standards, zinc die casting was selected to produce the housing and meet performance and...
strapad2_photo2_caseID186

Strap Adapter, Entry Slide Mount, Belt Sheave

View

Die casting the three components in ZA-27 alloy offers attractive aesthetics and a near-net shape, which eliminates machining costs. In addition, ZA-27 alloy provides good wear and bearing characteristics.