lowspee2_photo2_caseID103

Low-Speed, High-Load Bearings

View

The Champion Series IV grader incorporates ZA-12 alloy low-speed, high load bearing to improve operation performance. This Front Axle Bearing application acts as a replacement for the grader’s front axle needle bearings. The original needle bearings performed well...