Alloys: Zamak 5 (ZL5, ZL0410, ZnAI4Cu1, alloy 5)

ima13

Dental – Occlusal Bite Holder Block

View

The medical sector is a highly demanding, niche market. The main benefit of using zinc die casting for this product is the outstanding surface quality achieved.
ima11

Electronics Housing

View

SINAMICS Control Unit CU305  This casting is a housing for the most demanding industrial electronics. To avoid short circuits, it needs to be free of residual particles. To save costs for post-processing and cleaning steps, a net-shape mold concept was developed....
ima10

Bayonet XT-A

View

The 3-piece bayonet XT-A is assembled into a circular piece and provided with a cover plate. The part is designed so that it connects with an inlay heatsink, necessary due to the heat generated by the installed LED (60-80°C). The casting challenge is to achieve a...
ima09

Support Unit for Drive

View

This product is a segment drive for imaging plate technology used in dentistry. A complex, modern, and advanced die casting enables precise and optimum shape design that is consistent with the mechanical properties of the die cast zinc alloy. In medical technology,...
ima08

Central Support Unit

View

This part is a central support unit for mounting all optical, electrical, and mechanical components for the imaging plate technology in use in dentistry. In medical technology, die cast zinc has been used for many years; however, overall, this area of ​​application is...