Alloys: Zamak 3 (ZL3, ZL0400, ZnAI4, alloy 3)
View
This part, which replaced a machined steel part, required precision tolerances for the diameter of the bores and the spacing between them. Zinc casting also provided the required dimensional stability over time and permitted this complex shape to be cast in one piece...
View
The part is machined on guiding bores and reference faces. It substitutes for the pressed steel plate for several reasons: its high precision realized on machined diameters Ø < 0.02 mm and for the cost efficiency.
View
Initially, the hub–two intersecting cylinders–was a brazed assembly. Cylinders were screw machined from solid brass. Operations included turning, drilling, internal milling, cut-off, and rolling of one cylinder end to accept a plastic transition piece. The redesigned...
View
Ignition switch corrosion was the source of customer frustration and concern. Standard panel nuts, like the ones used to secure the ignition switch to the riding mower control panel, are made of stamped steel. The die cast company’s technical staff proposed changing...
View
This chassis for a motor drive unit for an automatic opening roller door was made from several pressed metal parts prior to being designed as a zinc die casting. Die casting in zinc alloy 3 provided numerous benefits: 1.) Additional features such as pockets, the...